Tony
I venture to suggest that what you have been doing is not cleaning but
rather a re-distribution of the contaminants over a wider area.
If you have to clean, then use a machine ....poetry, pure poetry!
Otherwise I would recommend using a no-clean that you can leave on safely
without cleaning - is there such a thing? I am not sure but it does depend
upon the operating conditions your assembly is working under.
Regards, Graham Naisbitt
[log in to unmask]
www.concoat.co.uk <http://www.concoat.co.uk>
For instant access to Product Data Sheets register on the Tech-Shot area of
www.concoat.co.uk <http://www.concoat.co.uk>
Concoat Limited
Alasan House, Albany Park
CAMBERLEY GU16 7PH UK
Phone: +44 (0)1276 691100
Fax: +44 (0)1276 691227
Mobile: +44 (0)79 6858 2121
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Tony Conlon
> Sent: Wednesday, June 13, 2001 02:36
> To: [log in to unmask]
> Subject: [TN] A solution to white residues after smt rework ...
>
>
> We're using:
> Kester #186 Flux Pen
> Microcares Vericlean (applied from aerosol can thru a hand-held brush)
>
> All our material is surface mount, no bga's,
> We run a no-clean process ...
>
> Problem: We clean after repair/rework for cosmetic reasons ... the cleaner
> we are using leaves a trace amount of white residue behind ...
>
> I have also tried Multicores Mini-Fluxers & Mini-Cleaner ... less residue
> ... non-consistant ... not 100% satisfied.
>
> Does anyone have a tried and trusted system?
> Regards,
> Tony.
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following
> message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|