No electrically conductive paint or adhesive is going to be anything like as
conductive as metal, typically by a couple of orders of magnitude. For
cheapness you might want to look at some of the carbon filled polymer inks
used in flex circuits, also outside the electronics industry conductive
coatings and adhesives are used in buildings/constructional applications.
These are to ensure electrical continuity in static sensitive facilities /
applications [like flour mills for example) and are typically based on
copper
Mike Fenner
Indium Corporation of Europe
-----Original Message-----
From: Peter tremewen [mailto:[log in to unmask]]
Sent: Wednesday, May 30, 2001 11:28 PM
To: [log in to unmask]
Subject: [TN] Conductive Paint......
Hi Techneters,
The current discusion about Conductive epoxy brings to mind a question I
had about conductive paint.
Does any one know where I might find a good reasonably cheap source of
conductive paint? The only source
I have found here in Australia is prohibitively expensive, and not very
conductive. Any sugestions would
be appreciated. The aplication is but low voltage and low amps, and designed
to be totally disposable if
a fault occurs, so low cost is an important consideration.
Thanks......
)O( )O( )O( )O( )O( )O( )O( )O( )O( )O( )O( )O( )O( )O(
The Sinister Dragon
Hey, Just because I'm EVIL,
Doesn't make me a bad person...... >:-)
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|