TECHNET Archives

May 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Graham Naisbitt <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 23 May 2001 12:06:20 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (77 lines)
Charles

As I recall, Solithane 113 was developed specifically for space applications
being NASA approved for no outgassing issues.

I would be surprised if you could spray coat for a  space application,
because you will increase the potential for outgassing problems by the
addition of thinners to make it "sprayable".

If you application is space related I recommend dip or brush only.

If it is not a space application, then you will find much more
"user-friendly" materials of a more conventional nature.

Regards, Graham Naisbitt

[log in to unmask]
www.concoat.co.uk

Concoat Limited                     www.concoat.co.uk
<http://www.concoat.co.uk>
Alasan House, Albany Park
CAMBERLEY GU16 7PH UK
Phone: +44 (0)1276 691100
Fax: +44 (0)1276 691227
Mobile: +44 (0)79 6858 2121



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of [log in to unmask]
Sent: Tuesday, May 22, 2001 05:57
To: [log in to unmask]
Subject: [TN] solithane conf. coat


I hope this one gets though. First thanks to all for the help you have given
and
the education I receive from the Technet. I have trouble responding in kind,
our
e-mail doesn't always let me reply.
 Now the question. Does anyone spray Solithane 113 conformal coat?  We are
currently brushing with it, but I have been asked to spray. Is there any
special
info I should know? We spray manually with a paint gun or an airbrush.
Thanks again ( especially my last question- soldering to stainless steel )
Fortunately I won't have to do that after all.

Charles Caswell
Process Lead, PCB
Frontier Electronic Systems

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2