Jim...far from muddy, Frank has this one right. The dense pile
construction of Duroid leaves a stringy edge after de-panelization. It
also requires a reduced web spec to avoid stress fracturing at the part
edge. We have done some of pwav's work....Frank is the maven on this one.
Mark Simmons
Marsico, James wrote:
> Hello Technet... a quick question. Are Teflon boards (Duroid) a good
> candidate for scoring? What would be the best method for panelized assembly
> and singulation?
> Thanks in advance,
> Jim Marsico
> Senior Engineer
> Production Engineering
> EDO Electronics Systems Group
> [log in to unmask] <mailto:[log in to unmask]>
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
>
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|