The Uresolve Plus SG that I had mentioned only takes 10-15 minutes depending
upon solvent temperature, and thickness of deposit, etc.

On the plus side (no pun intended), you can pull it out at any time to view
the status.

Another plus is that it is relatively non-toxic to work with (unlike MEK,
etc.), but I still would use normal precautions to avoid exposure when
handling.

Steve Creswick
Gentex Corporation

-----Original Message-----
From: Mike Fenner [mailto:[log in to unmask]]
Sent: Tuesday, May 08, 2001 1:42 PM
To: [log in to unmask]
Subject: Re: [TN] Removing epoxy encapsulation


There is a company out there that supplies a piece of equipment for
doing exactly this, but can't remember what its called. Basically it
squirts a jet of concentrated acid, [another way of doing this which
uses an abrasive jet]. Both need some care. Suggest try contacting the
guys that supply wire/diebonders etc, they move in the s/c back end
and hybrid assembly worlds and are likely to be familiar with this
type of requirement. Alternatively just dunk in one of the solvents
already suggested and be p  a t  i  e  n t zzzz...


Mike


----- Original Message -----
From: "Stephen R. Gregory" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, May 08, 2001 5:11 PM
Subject: [TN] Removing epoxy encapsulation


> Hi ya'll!
>
> Could anybody tell me what kind of chemical/solvent I could use to
remove
> epoxy encapsulation material? What I'm trying to do is look at the
wire bonds
> on some failed tunnel diodes...
>
> Thanks!
>
> -Steve Gregory-
>
> --------------------------------------------------------------------
-------------
> Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
> To unsubscribe, send a message to [log in to unmask] with following
text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> --------------------------------------------------------------------
-------------
>

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2