Sorry, I don't know the brand, but about 1963 I saw this done to inspect
the spot welds in an epoxy potted module on a satellite command decoder
module. It took about two weeks of soaking in a rather vile solution
and we had to pick at it from time to time to flake off the softened
epoxy.
Don't give up, it is (was) out there somewhere. As I recall we were
buying our stuff from Dow-Corning at that time.
Also, consider X-Raying it.
Bob Smith
Stephen R. Gregory wrote:
>
> Hi ya'll!
>
> Could anybody tell me what kind of chemical/solvent I could use to remove
> epoxy encapsulation material? What I'm trying to do is look at the wire bonds
> on some failed tunnel diodes...
>
> Thanks!
>
> -Steve Gregory-
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
--
--------- Avoid computer viruses -- Practice safe hex -------------
* * Specializing in small, cost effective embedded control systems * *
Robert L. (Bob) Smith Smith Machine Works, Inc.
internet [log in to unmask] 9900 Lumlay Road
landline 804/745-1065 Richmond, Virginia 23236+1004
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|