TECHNET Archives

May 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Ingemar Hernefjord (EMW)" <[log in to unmask]>
Date:
Tue, 15 May 2001 09:35:50 +0200
MIME-Version:
1.0
X-To:
Genny Gibbard <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Ingemar Hernefjord (EMW)" <[log in to unmask]>
Parts/Attachments:
text/plain (87 lines)
Our companies have been using hundreds of tons of Tin and Lead and the company has  made many millions of boards and still few have ever seen whiskers on a PWB. It seems to me that whiskers occur more frequently on components, on terminals, on leads, wires, washers, contacts,  connectors and other parts with mixed geometries, bends, mixed materials, irregularities and structures that are not like the 'singularity' of  PWBs. It also seems as forces that develop in the construction (e.g. large CTE mismatch) will enhance the creation of whiskering. I have tried to understand what Jong and others have written in the matter, and it all seems to be something that occurs on atom level rather than in the understandable and visible macro world. All that I have found seems to be based on empirical runs with different Tin thickness (Jong means that thinner than 0.5 microns= no problem / thicker than 10 microns= no problem)and varying Lead alloying (Jong means adding 1-3% Lead eliminate!
s whiskering)but no deeper thermodynamic or chemical or other studies seem to have been done. So, if we don't know the basic driving mechanism we will still get surprises, don't we?

Ingemar Hernefjord
Ericsson Microwave Systems


-----Original Message-----
From: Genny Gibbard [mailto:[log in to unmask]]
Sent: den 14 maj 2001 20:47
To: [log in to unmask]
Subject: Re: [TN] Pure Tin


Well, that's just the thing - is whiskering non-existent with lead in the
mix?  The article in the advanced packaging magazine said that lead had
nothing to do with reducing or eliminating whiskers, that tin could whisker
even when mixed with lead and they had a couple of pictures as examples.
Their premise was more about that better processes have reduced or
eliminated the whiskering and that is the only reason why we see less
whisker problems today.  They said that Tin should be considered a simple
drop in replacement for tin-lead.

I get a little concerned when someone seriously contradicts an organization
like NASA, not that NASA can't be wrong.  But it looks like NASA has thrown
a lot of money at the problem, so why haven't they ever come across the
problem of tin-lead having just as much propensity to whisker as straight
tin?

As far as the boards we received, I'm pretty sure they are a white tin, and
I'm sure that they would work fine for the uses they are designed, but it is
a concern when a co. just substitutes one process for another without
telling you.  It is questionable whether we will use that co. again.

-----Original Message-----
From: George Milad [mailto:[log in to unmask]]
Sent: May 14, 2001 12:10 PM
To: [log in to unmask]
Subject: Re: [TN] Pure Tin


Genny,
If your supplier has used immersion tin as a solderable finish; then you
should be able to assemble  the parts successfully.
After assembly the immsersion tin is disolved into the solder and becomes
part of the solder joint.  Immersion tin as such would cease to be part of
the finished product, and the probability of "Solder Whiskering" is non
existent.
I hope this is helpful.
George Milad
Shipley Ronal Inc

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2