From what I gather from your description, I have battled this exact problem
at a previous employer. Although this may be different from your process, it
turned out for us that the initial rinse temperature of our wash system was
too high. To make a long story short, we lowered the temperature of the
first zone by about 20 degrees F and never had the problem again.
Jon Moore
---------------------------------------------------------------------------------