Janice
I have limited experience with solder balls but I have seen a 'wrinkling' of the surface. If
you let me have a picture then I can tell you whether it is the same as I saw.
I have come across a number of hypotheses as to the cause - oxidation and differential cooling
of the solder being two. I do not think that it causes any problems that might be associated
with the physical properties of the ball.
Michael McInerney
"Pelchat, Janice" wrote:
> We have some ceramic BGAs that are giving us problems with fractures at the
> ball/package interface after reflow.
>
> In the process of failure analysis, we inspected unassembled parts under
> high power and have seen two anomalies. One is an apparent shaving of the
> outside perimeter balls from what appears to be fixturing at the
> manufacturer - that is being F/Ad by the manufacturer. The other anomaly is
> what I can only term a "star" shaped appearance on the surface of the
> solderballs.
>
> Under very high power, this "star" effect seems (to me at least) to be the
> result of the solidification process of the solderball during manufacture.
> It looks as though the solder surface separated - then the separations
> formed crevices in a star pattern. Think of the appearance of crevices
> formed on crusty breads when they bake and cool. (Sorry for the analogy -
> in my other life - I bake).
>
> I have a fair picture for those wanting to see a visual. Does this sound
> familiar to anyone? Is it part of the normal BGA solderball appearance?
>
> Jan Pelchat
> Benchmark Electronics
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|