Paul,
We have had similar problems coating similar connectors. Our solution was
to place a "dam" of non-corrosive RTV around the base of the connector to
keep the Humiseal from entering the connector.
HIH,
Roger M. Stoops, C.I.D., PCB Designer
Trimble
Engineering and Construction Division
5475 Kellenburger Rd.
Dayton, OH 45424-1099 USA
Ph: +01 937.233.8921 or +01 937.233.4574 ext 288
Fax: +01 937.233.7511
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|