Frank: As I recall the Minico M-1012-RS is a hundred ohm/sq phenolic carbon
resistor material.
We have used a variety of Minico products in the past. We have replaced
these with products from Tamura and Electra for our screened resistor
applications. Both have worked well for us. Info on these should be
available on the web.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: Frank Barber [mailto:[log in to unmask]]
Sent: Wednesday, May 02, 2001 10:33 AM
To: [log in to unmask]
Subject: [TN] Fixed Carbon Resistors
I have a question,
We used to purchase a product from Emerson & Cuming, Inc. called
"MINICO M-1012-RS" which is a screened resistive ink. Our supplier no
longer carries this product. Does anyone know where we maybe able to locate
a new supplier that offers this type of product? Thanks in advance.
Franklin D. Barber
Special Projects Engineer
Modular Component National, Inc.
2302 Industry Court
Forest Hill, MD 21050
Phone: 410-879-6553
Fax: 410-838-7629
Email: [log in to unmask] <mailto:[log in to unmask]>
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|