TECHNET Archives

May 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
quoted-printable
Sender:
Subject:
From:
"d. terstegge" <[log in to unmask]>
Date:
Tue, 1 May 2001 13:21:52 +0200
Content-Type:
text/plain; charset=US-ASCII
MIME-Version:
1.0 (Generated by NET-TEL Mailguard SMTP version 4.0.0.22)
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "d. terstegge" <[log in to unmask]>
Parts/Attachments:
text/plain (42 lines)
We test cleanliness on a daily basis, with a randomly selectedboard that happens to be in production that day. We put the measuring-results in an SPC chart. But in reality, what we measure is variations in board type, and in the way these boards were assembled (wavesolder yes or no, time between process steps, cleanliness of components). It doesn't make sense to do statistics on these data.
So for SPC I very much like the idea of using only one standard testboard, since it eliminates most (not all) of the variables.
But I would use this method IN ADDITION to sample based measurements, and not instead of it, for the reasons already stated by others.

Kind regards,

Daan Terstegge
Unclassified mail
Personal Website: http://www.smtinfo.net


>>> Lou Hart <[log in to unmask]> 04/30 7:35 pm >>>
TechNetters, I'm following up on a discussion we had some months back,
regarding use of an Omegameter at the end of a cleaning operation for SPC.

Our production manager asked if we could use a single, standard board, run
it through the solder wave and cleaner, then test it in the omegameter,
doing this at prescribed time intervals for SPC.  Let me make sure I'm
clear:  this standard board would be one unit, that would be used
repeatedly to check the cleaning operation.  Using the single, standard
board would eliminate variablity from handling, board and material
composition, and all the things that affect the omegameter reading.  The
only variables (we speculate) would be in the solder wave and the cleaner,
the latter of which we are wanting to control.

What, if anything, is wrong with this idea?

My understanding is that incompletely cured laminate can release ionic
material.  Could there be any such problem with solder resist?

Lou Hart

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2