IMO you should use the same alloy that you use for your reflow process. I
wouldn´t go with something special.
If you´re in need of putting non eutectic balls on that device - I can´t
suggest a tool ( haven´t done it myself ).
For eutectic balls you don´t need preformed balls, there´s a tool, for
example from WELLER, to print paste on the device and than reflow that
arrangement to form the balls.
Hope that helps a bit
Wolfgang
-----Ursprüngliche Nachricht-----
Von: Van Hoang Dinh [mailto:[log in to unmask]]
Gesendet am: Dienstag, 22. Mai 2001 07:19
An: [log in to unmask]
Betreff: [TN] Re-ball BGA
Hi all,
I got few questions about reballing the BGA.
1. If I want to re-ball the BGA, so what's alloy should use for the
balls???63/37 or 60/40 or ....
2. what's method should i use to placing the balls on the BGA if the balls
are in loose form ???
3. what ' s profile should I use for reflow the BGA's???
Thanks for your help
Van
[log in to unmask] <mailto:[log in to unmask]>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|