TECHNET Archives

May 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
"<Peter George Duncan>" <[log in to unmask]>
Date:
Mon, 21 May 2001 08:09:10 +0800
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (79 lines)
Hi, Steve,

Are you sure the URL is correct? I get a message saying "The requested URL
was not found on this server" - any update for the current location?

Pete Duncan





                    "Stephen R.
                    Gregory"             To:     [log in to unmask]
                    <SteveZeva@AO        cc:     (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
                    L.COM>               Subject:     Re: [TN] Black Pad
                    Sent by:
                    TechNet
                    <[log in to unmask]
                    ORG>


                    05/18/01
                    09:00 PM
                    Please
                    respond to
                    "TechNet
                    E-Mail
                    Forum.";
                    Please
                    respond to
                    SteveZeva






Hi Guenter!

There's real good article about Black Pad that was presented at the 1999
Printed Circuits Expo thas has all kinds of good pictures. It's at:

http://www.nukcg.org/downloadfiles/Hadco%20on%20Immersion%20Gold%20failures.pd

f

-Steve Gregory-


 Quite a while ago there was a discussion in TechNet about Black Pad. I
 read
 some articles too, but what I am missing is a picture or two or so how
 Black pad looks like ( sure it's more than just black ).

 Have a great day

 Guenter

 Guenter Grossmann

 Swiss Federal Institute for Materials Testing and Research EMPA
 Centre for Reliability
 8600 Duebendorf
 Switzerland

 Phone: xx41 1 823 4279
 Fax :      xx41 1823 4054
 mail:     [log in to unmask]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2