BTW... we've been using HF flux for well over 5 years and wouldn't think of
changing.
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
-----Original Message-----
From: Brian Ellis [SMTP:[log in to unmask]]
Sent: Friday, May 18, 2001 2:26 AM
To: [log in to unmask]
Subject: Re: [TN] Rework Wires and OA Flux
Doug
Citric acid is a funny one. It is tribasic (compared with dibasic
for
most of the other usual N/C activators). Hughes are not the only one
to
come unstuck with citric: Zeva had a citric acid/glycerol (a triol
or
tribasic alcohol) W/S flux in the 1970s, long before Hughes. I
believe
that the problem with citric is that it forms unstable chelates with
some heavy metals (don't drink lemonades etc. from lead crystal or
lead-containing pewter vessels!). The later formulations were, I
believe, with maleic acid (found in green apples), which is dibasic.
Its
ages since I heard anything about HF fluxes: I thought they had died
a
natural death.
I had a really bumper crop of lemons this winter, so my personal
citric
to maleic ratio has increased enormously :-)
Brian
Douglas Pauls wrote:
>
> Very interesting, Jim. Do you happen to know who made the HF
series of
> fluxes? I would like to get data sheets on them.
>
> The original HF1189 was based on citric acid (lemon juice) as the
> activator. The HF stood for Hughes Flux. When it first came out,
it was
> hailed as the greatest thing since sliced bread. A classic case
of a
> marketing department gone amuck. The citric acid can be corrosive
and
> there were some memorable military failures as a result. Several
studies
> were done on the 1189.
>
> I believe Kester picked up the 1189 family. They reformulated the
> activator away from citric acid toward more benign weak organic
acids and
> called it HF1189A. If I recall, the 1189A contains no citric
acid.
>
> I suggest you contact Kester for more information.
>
> Doug Pauls
> Rockwell Collins
>
>
----------------------------------------------------------------------------
-----
> Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
> To unsubscribe, send a message to [log in to unmask] with following
text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following
message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
>
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|