Doug,
**Assume I do not have the option of using a no clean flux.
*And why would I be making such an assumption? A low solids flux is your
best answer.
Well, QA is queasy about trying to explain to a customer why there is
residue on the board when the customer is not used to seeing it. I don't
know, sometimes it is very hard to make progress. Personally, I like the no
clean flux option. I have never been a fan of local cleaning as it is not
truly effective. I will keep hammering away!
Thanks for your input.
Bob
Robert Barr
Manufacturing Engineering
Formation, Inc.
Voice: 856-234-5020 x3035
Fax: 856-234-6679
email: [log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|