This may or may not be useful, (probably a mental file away just in
case). In a previous existence we did some work on cutting various
Duroids with CO2 lasers. The results were excellent, with very clean
accurate edges no tearing or vertical displacements of tracking etc.
Our customer -working on very high frequency rf stuff - was delighted.
The bad news was in two related areas:
1) IT was fairly costly compared to mechanical cutting.
2) The tracking on the boards was not as accurate as our laser tables,
with cumulative errors on the circuits across the panel in particular,
in both x and y and even theta on some, naturally this added further
to cost as this meant we had to reset for each circuit in the panel.
Probably some of this was due to some dimensional instability in the
Duroid, and some to the fact we were observing tolerances called out
in drawing but the original fabricator was not.
Mike Fenner
----- Original Message -----
From: "Frank Kimmey" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, May 15, 2001 3:41 PM
Subject: Re: [TN] SCORING TEFLON BOARDS
> Hey Jim,
>
> Scoring of Teflon PWAs can be done but care must be taken during
> depanelization. You will likely see an ugly edge (exposed fibers,
etc.)
> unless you use a sharp cutter (I have seen Teflon pass through the
> "pizza-wheel" style depanelizers with no effect, the laminate was
soft
> enough to squish through and not separate). IMHO only tab routing
should be
> used with exotics (Teflon, Ceramics, etc.) otherwise you will not
get a
> consistent clean edge and may experience de-lam due to
depanelization. Give
> me a call if I can muddy the subject up more.
> Hope it helps,
> FNK
>
> Frank N Kimmey, C.I.D.
> Senior PCB Designer
> Powerwave Technologies
> PH. 916-941-3159
> Fax 916-941-3195
>
>
> -----Original Message-----
> From: Marsico, James [mailto:[log in to unmask]]
> Sent: Tuesday, May 15, 2001 7:07 AM
> To: [log in to unmask]
> Subject: [TN] SCORING TEFLON BOARDS
>
>
> Hello Technet... a quick question. Are Teflon boards (Duroid) a
good
> candidate for scoring? What would be the best method for panelized
assembly
> and singulation?
> Thanks in advance,
> Jim Marsico
> Senior Engineer
> Production Engineering
> EDO Electronics Systems Group
> [log in to unmask] <mailto:[log in to unmask]>
>
> --------------------------------------------------------------------
--------
> -----
> Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
> To unsubscribe, send a message to [log in to unmask] with following
text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message:
SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources &
Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
> ext.5315
> --------------------------------------------------------------------
--------
> -----
>
> --------------------------------------------------------------------
-------------
> Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
> To unsubscribe, send a message to [log in to unmask] with following
text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> --------------------------------------------------------------------
-------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|