Hey Jim,
Scoring of Teflon PWAs can be done but care must be taken during
depanelization. You will likely see an ugly edge (exposed fibers, etc.)
unless you use a sharp cutter (I have seen Teflon pass through the
"pizza-wheel" style depanelizers with no effect, the laminate was soft
enough to squish through and not separate). IMHO only tab routing should be
used with exotics (Teflon, Ceramics, etc.) otherwise you will not get a
consistent clean edge and may experience de-lam due to depanelization. Give
me a call if I can muddy the subject up more.
Hope it helps,
FNK
Frank N Kimmey, C.I.D.
Senior PCB Designer
Powerwave Technologies
PH. 916-941-3159
Fax 916-941-3195
-----Original Message-----
From: Marsico, James [mailto:[log in to unmask]]
Sent: Tuesday, May 15, 2001 7:07 AM
To: [log in to unmask]
Subject: [TN] SCORING TEFLON BOARDS
Hello Technet... a quick question. Are Teflon boards (Duroid) a good
candidate for scoring? What would be the best method for panelized assembly
and singulation?
Thanks in advance,
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|