Yes, Colin. We use 4.5 microinches of Gold over 150 microinches of Nickel
to obtain a flat surface for our 388 pin 1.27mm pitch PBGA's. Owing to the
thick Nickel layer, we have to use a high melting point tin/lead solder
with about 2% silver to get the finish we want from the joints.
Regards
Pete Duncan
Colin Weber
<colin.weber@VARI To: [log in to unmask]
ANINC.COM> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST
Sent by: TechNet Group)
<[log in to unmask]> Subject: [TN] Surface Finish for 1.27mm PBGA
05/10/01 09:45 AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to Colin
Weber
Could anyone inform me of whether an Electroless Gold surface finish which
conforming to IPC-6012 Class3, is suitable for a 388pin PBGA of 1.27mm
pitch?
Regards,
Colin Weber
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|