Peter,
Thanks for sharing your results with us. Knowing about this stuff is good
info to have in one's back pocket. I do feel vindicated though in that the
stuff does not wholesale dissolve the cured silicones.
Bev Christian
Research in Motion
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: April 3, 2001 1:40 AM
To: TechNet E-Mail Forum.; Bev Christian
Subject: Re: [TN] Solvent for RTV738
Bev and other interested TechNetters,
FYI, I ran some trials a couple of days ago with Dynaloy's Dynasolve 218
and 711 to remove the RTV738 that was causing us a problem. These chemicals
are termed 'Silicone Solvents', but for cured Silicones, you shouldn't
expect them to disappear nicely into solution. They won't. Not in anybody's
lifetime, at least.
The 711 solvent worked best, after heating it on a coffee maker to 90
degrees C (or whatever temperature the thing makes coffee at), though it
was recommended that it be heated to 125 degrees. It was applied to room
temperature boards with a cotton bud (Q-tip, I believe, to my American
cousins) in quantities sufficient to thoroughly wet the sealant, but
without soaking the surrounding countryside. After 2 to 3 minutes, the
edges of the sealant were massaged with the cotton bud to lift them and
permit the solvent to penetrate underneath.
After a further 5 to 10 minutes, the sealant could be peeled off quite
cleanly. The trial board was then washed thoroughly in alcohol, followed by
a water wash and examined for any corrosion damage. None was evident. The
board was FR4 with a variety of ceramic and plastic components. Care was
taken to avoid trimpots and DIP switches, but the viscosity of the solvent
is greater than that of water, so its powers of penetration are limited.
The solvent is quite an effective paint stripper, so watch out for that if
you're thinking of using it anywhere where you value the paintwork. For me,
though, it was a good result, and my thanks to Jeff Gerarden for suggesting
Dynasolve.
Pete Duncan
----- Forwarded by DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group on 04/03/01
01:17 PM -----
DUNCAN Peter
To: "TechNet E-Mail Forum."
<[log in to unmask]>, Bev Christian
03/23/01 06:17 <[log in to unmask]>
PM cc:
Subject: Re: [TN] Solvent for
RTV738(Document link: DUNCAN Peter)
Bev,
The company is Dynaloy.com.
Rgds
Pete
Bev Christian <[log in to unmask]>@IPC.ORG> on 03/22/2001 09:16:00 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Bev Christian <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: Re: [TN] Solvent for RTV738
Jeff,
1) I tried Dynasolve.com and was not taken to their web page.
2) Are you saying that this stuff will dissolve cured or uncured
silicones?!
Bev Christian
Research in Motion
-----Original Message-----
From: Gerarden, Jeff [mailto:[log in to unmask]]
Sent: March 22, 2001 2:57 AM
To: [log in to unmask]
Subject: Re: [TN] Solvent for RTV738
If this material is a silicone I have used Dynasolve 225 to dissolve the
Dow
Corning RTV on several PCB's with great success. You could find the company
on the web by typing the product name above. Make sure you look at the
technical data sheet on this material. Hope this helps you out.
> Jeff Gerarden
> Focus Factory Supervisor
> PLEXUS-ELECTRONIC ASSEMBLY CORP.
> 2121 Harrison St. Neenah WI 54956
> phone: (920) 751-3226
> email: [log in to unmask]
> http://www.plexus.com
>
>
> -----Original Message-----
> From: <Peter George Duncan> [SMTP:[log in to unmask]]
> Sent: Tuesday, March 20, 2001 8:12 PM
> To: [log in to unmask]
> Subject: [TN] Solvent for RTV738
>
> Hi, TechNetters,
>
> I am trying to find a solvent for removing 3M's RTV 738 that has been
used
> for bonding components to a number of boards, or to each other. Any
> suggestions?
>
> I have tried 3M themselves and they have no solvent of their own apart
> from
> "Citrus Base Adhesive Remover" that 'may soften' it enough to peel it
off,
> but this seems pretty indefinite.
>
> Thanks in hope
>
> Pete Duncan
> Asst Principal Engineer
> Singapore Technologies Aerospace
>
>
--------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases
>
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
>
--------------------------------------------------------------------------
> -------
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|