Can anybody recommend a solder paste vendor
with the following compostion:
1. 15Sn/82.5Pb/2.5Ag 85 % metal loading (For
Dispensing - 500 +635)
2. 5Sn/93Pb/2Ag. 85 % metal loading (For
Dispensing -500 + 635)
I need this paste for our manufacturing.
Thanks for your help
---------------------------------------------------------------------------------