Hi Bev,
I am not aware of any specific study, but Ag is actually worse than Au (see
1983-88 IEEE Compliant Lead Task Force papers--not too many and very
incomplete because of legal problems), but no critical percentage is known.
Thus, Ag+Au may actually be worse than Au.
Werner Engelmaier
---------------------------------------------------------------------------------