TECHNET Archives

April 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"Tempea, Ioan" <[log in to unmask]>
Date:
Fri, 6 Apr 2001 12:24:31 -0400
Content-Type:
text/plain
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Tempea, Ioan" <[log in to unmask]>
Parts/Attachments:
text/plain (35 lines)
Hi technos,

and big thanks for the interest in my problem. Now, I tried to follow all
the leads, I checked the solder mask, I ruled out the contamination, since
the problem shows on each and every board, checked for oily residues, etc.

To clarify, the problem pads show no sign of having been in contact with the
solder, they are like before waving.

So I still can't put the finger on the cause. However, by hand spraying the
bottoms, or running the foam fluxer at max, we reduced the number of
problems. We even get, from time to time, fully soldered boards.

Maybe the boards have gone through some thermal cycling that made the
intermetallics grow, or the pads are oxidized for some reason. Maybe a bad
batch. I'm sure that a stronger flux would solder very well, but why this
deviation from the regular process, since we are talking regular boards?

So, the follow up question is:
what should I do to avoid that the problem reappear while running a future
job, eventually high volume?

Thanks,
Ioan

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2