TECHNET Archives

April 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Graham Collins <[log in to unmask]>
Date:
Mon, 30 Apr 2001 14:10:11 -0400
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Graham Collins <[log in to unmask]>
Parts/Attachments:
text/plain (42 lines)
Lou
First off - you are worried about what you build today, not a "standard" board.  Let's say you have your standard board, but then your pwb vendor does something unusual and ships you some boards with nasty chemicals on them - you won't test them so you will never notice.  If you run a no-clean process - very dangerous.

But more importantly, running the "standard" board through the assembly operation will degrade it over time - we have boards used repeatedly for thermal profile verification and they gradually deteriorate.  So your solder mask would change in characteristics, and thus your results can not be relied upon.

regards

Graham Collins
Process Engineer, Litton Systems Canada, Atlantic Facility
(902) 873-2000 ext 6215

>>> [log in to unmask] 04/30/01 02:35PM >>>
TechNetters, I'm following up on a discussion we had some months back,
regarding use of an Omegameter at the end of a cleaning operation for SPC.

Our production manager asked if we could use a single, standard board, run
it through the solder wave and cleaner, then test it in the omegameter,
doing this at prescribed time intervals for SPC.  Let me make sure I'm
clear:  this standard board would be one unit, that would be used
repeatedly to check the cleaning operation.  Using the single, standard
board would eliminate variablity from handling, board and material
composition, and all the things that affect the omegameter reading.  The
only variables (we speculate) would be in the solder wave and the cleaner,
the latter of which we are wanting to control.

What, if anything, is wrong with this idea?

My understanding is that incompletely cured laminate can release ionic
material.  Could there be any such problem with solder resist?

Lou Hart

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2