Phil
Above all, do not be misled into thinking that silicone materials, being
rubbery, will transmit shock less. Nothing is farther from the truth:
many silicone rubbers are almost totally incompressible in the short
time scale. Any mechanical energy imparted to it by a short duration
shock will be dissipated almost entirely within the components, to their
obvious detriment (super-bouncing ball effect, where almost no kinetic
energy is dissipated in the rubber, allowing it to rebound multiple
times).
Brian
DUTTON Phil wrote:
>
> Hello Technetters,
>
> I am soon to design a PB for one of our customers that will be required to
> withstand a shock load of approximately 1500 g's.
> Does anyone have any guidelines or advice on how to achieve this?
> I'm thinking of solid potting the assembly within a rigid structure as one
> solution.
> Components are expected to include SMD discretes and BGAs.
> Of course there's the consideration of how hard the potting compound needs
> to be and what it should be (epoxy, silicone elastomer), as well as what
> material the board should be made of, CTE considerations between the board -
> components - compound - housing etc.
> Any advice would be most welcome.
>
> Phil Dutton C.I.D.
> Senior CAD Technician
> IPC Certified Interconnect Designer
>
> Tenix Defence Systems Pty Ltd
> Systems Division - Adelaide
> Second Avenue, Technology Park,
> Mawson Lakes. SOUTH AUSTRALIA 5095
>
> ================================
> Phone (08) 8300 4400 (reception)
> (08) 8300 4481 (direct)
> Fax (08) 8349 7420
> email [log in to unmask]
> Internet Page http//www.tenix.com
> ================================
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|