Russell,
Among others, you can contact MIcrolapp Technologies of Rolla, ND at
http://www.microlap.com/. I dealt with a gentlemen named Terry Hoselton 4
or 5 years back. Not sure if he is still there. It was a good place for
custom zirconia ferrules and split sleeves. See if he remembers Steve
Creswick from CTS in West Lafayette.
Steve Creswick - Gentex Corp
-----Original Message-----
From: Russell Epstein [mailto:[log in to unmask]]
Sent: Friday, April 20, 2001 3:26 PM
To: [log in to unmask]
Subject: [TN] What companies can grind ceramic ferrule blanks
I have a very large supply of fiber optic ferrule blanks and I am
looking to have them ground or possibly wholesale them off.
--
Russell Epstein
President
Advanced Industrial Ceramics
12651 Briar Forest Dr.
Houston, Tx 77077
[log in to unmask]
Tel: 281-497-4788
Fax: 281-556-9244
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|