TECHNET Archives

April 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
IPC DesignerCouncil <[log in to unmask]>
Date:
Thu, 19 Apr 2001 20:38:32 +0200
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "F.Pitzl" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
"F.Pitzl" <[log in to unmask]>
Parts/Attachments:
text/plain (26 lines)
Hello,

At this day I was asked by our engineer if it is possible to put a
additional silk-screen onto the board.
This additional silk-screen has to be in a different color than the
board and the normal one. Even it should have the same clearance and
minimal line width requirements as a Solder Mask. For this it must be a
photoimageable process.

What would you say to this issue ?
Is it possible to run a second "SolderMaskProcess" with a different Mask
and color and how much would it cost on your opinion ?

Regards,
Florian Pitzl

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2