Paul
Ideally, a "no-clean" residue is meant to be just that. The chemistry is
designed for the residues to be as innocuous as possible if left on. If
you wish to clean, then use a chemistry which is designed for that.
That having been said, it is **sometimes** possible to clean "no-clean"
but you should use compatible chemistry, usually employing some strong
components. For example, the Vigon A200 saponifier can sometimes do the
job with the right equipment and the right flux.
Brian
Paul Gill wrote:
>
> Hi All,
>
> I am searching for information about solvents to remove no-clean residue.
>
> The appearance is that of a white residue. I don't know the composition of
> the residue.
>
> Any help would be appreciated.
>
> Thanks
>
> Paul Gill
> Senior Process Development Engineer
> Finisar Corporation
> (408) 541 5626
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|