Steve/Shawn,
So how normally cured epoxy looks like? If you can post both, quick curing
v/s slow curing (regular) photos that will add more value to overall
discussion.
re,
ken patel
-----Original Message-----
From: Stephen R. Gregory [mailto:[log in to unmask]]
Sent: Tuesday, April 10, 2001 2:53 PM
To: [log in to unmask]
Subject: [TN] Caps shorting...thanks everyone!!
Hi all!!
Thanks for all the inputs! You guys hit the nail on the head! Shawn Murphy
sent me some pictures of how I could tell if the epoxy was cured too
quickly,
and our boards look exactly like the pictures. You can see for yourself the
pictures he sent me (he said I could post them on my X-drive):
http://www.xdrive.com/share/986939149898eWG8FXWxfiw3qZBzMyak
http://www.xdrive.com/share/986939109974A5ZJOjj0gMEnvZG7LePU
Again thanks everybody!!
(gawd this list is great!)
-Steve Gregory-
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|