Graham, Jeff and others,
Jeff and the manufacturer's web page say "dissolve". Graham and others say
soften and swell. As a chemist I see a BIG difference between those two
descriptions. I have always expected that the latter description is what
happens. Just for clarity, the definition of dissolve from the
Merriam-Webster On-line Dictionary is "to cause to pass into solution", as
in table salt dissolving in water. If the latter is correct, then I can keep
my shorts in my pants.
Anybody else want to wade into this one. Jeff, comments?
regards,
Bev Christian
Research in Motion
-----Original Message-----
From: Graham Naisbitt [mailto:[log in to unmask]]
Sent: March 23, 2001 12:03 PM
To: TechNet E-Mail Forum.; Bev Christian
Subject: RE: [TN] FW: [TN] Solvent for RTV738
Bev,
Please, do not eat your shorts!
This "stuff" quoted as a "hydrocarbon" should soften and swell but not
dissolve silicone. It will soften it enough to facilitate its removal,
although getting the itty bitty bits out from under the components will
require a fair degree of manual dexterity.
There are some true silicone digesters out there, but anything that will
truly dissolve or digest silicone, is not the sort of "stuff" you want to
mess around with unless you REALLY have to.
Regards, Graham Naisbitt
[log in to unmask]
www.concoat.co.uk
Concoat Limited www.concoat.co.uk
<http://www.concoat.co.uk>
Alasan House, Albany Park
CAMBERLEY GU16 7PH UK
Phone: +44 (0)1276 691100
Fax: +44 (0)1276 691227
Mobile: +44 (0)79 6858 2121
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Bev Christian
Sent: Thursday, March 22, 2001 04:50
To: [log in to unmask]
Subject: [TN] FW: [TN] Solvent for RTV738
Below is a message from Jeff Geraden that I thought I should share with all
of you.
Is it your collective opinion that I should now eat my shorts? :) Now I
want to know HOW this stuff works, even though I don't need to dissolve any
silicones right now.
Bev Christian
Research in Motion
-----Original Message-----
From: Gerarden, Jeff [mailto:[log in to unmask]]
Sent: March 22, 2001 11:36 AM
To: 'Bev Christian'
Subject: RE: [TN] Solvent for RTV738
Bev,
This material I know will dissolve Dow Corning 3145 from previous
experience. I am confident it will on other cured silicone RTV's. I forgot
to specify cured or uncured. I used the Dynasolve 225 and did not use any
other dynasolve choices. Make sure you obtain a Technical Data Sheet before
use. Some very important/good information on it.
http://www.dynaloy.com/dynasolve200series.htm
>
>
> Jeff Gerarden
> Focus Factory Supervisor
> PLEXUS-ELECTRONIC ASSEMBLY CORP.
> 2121 Harrison St. Neenah WI 54956
> phone: (920) 751-3226
> email: [log in to unmask]
> http://www.plexus.com
>
>
> -----Original Message-----
> From: Bev Christian [SMTP:[log in to unmask]]
> Sent: Thursday, March 22, 2001 7:16 AM
> To: 'TechNet E-Mail Forum.'; 'Gerarden, Jeff'
> Subject: RE: [TN] Solvent for RTV738
>
> Jeff,
> 1) I tried Dynasolve.com and was not taken to their web page.
> 2) Are you saying that this stuff will dissolve cured or uncured
> silicones?!
>
> Bev Christian
> Research in Motion
>
> -----Original Message-----
> From: Gerarden, Jeff [mailto:[log in to unmask]]
> Sent: March 22, 2001 2:57 AM
> To: [log in to unmask]
> Subject: Re: [TN] Solvent for RTV738
>
>
> If this material is a silicone I have used Dynasolve 225 to dissolve the
> Dow
> Corning RTV on several PCB's with great success. You could find the
> company
> on the web by typing the product name above. Make sure you look at the
> technical data sheet on this material. Hope this helps you out.
>
> > Jeff Gerarden
> > Focus Factory Supervisor
> > PLEXUS-ELECTRONIC ASSEMBLY CORP.
> > 2121 Harrison St. Neenah WI 54956
> > phone: (920) 751-3226
> > email: [log in to unmask]
> > http://www.plexus.com
> >
> >
> > -----Original Message-----
> > From: <Peter George Duncan> [SMTP:[log in to unmask]]
> > Sent: Tuesday, March 20, 2001 8:12 PM
> > To: [log in to unmask]
> > Subject: [TN] Solvent for RTV738
> >
> > Hi, TechNetters,
> >
> > I am trying to find a solvent for removing 3M's RTV 738 that has been
> used
> > for bonding components to a number of boards, or to each other. Any
> > suggestions?
> >
> > I have tried 3M themselves and they have no solvent of their own apart
> > from
> > "Citrus Base Adhesive Remover" that 'may soften' it enough to peel it
> off,
> > but this seems pretty indefinite.
> >
> > Thanks in hope
> >
> > Pete Duncan
> > Asst Principal Engineer
> > Singapore Technologies Aerospace
> >
> >
> --------------------------------------------------------------------------
> > -------
> > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> > To unsubscribe, send a message to [log in to unmask] with following text
> in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt delivery of Technet send the following message: SET
> > Technet NOMAIL
> > Search previous postings at: www.ipc.org > On-Line Resources & Databases
> >
> > E-mail Archives
> > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> > additional
> > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> > ext.5315
> >
> --------------------------------------------------------------------------
> > -------
>
> --------------------------------------------------------------------------
> --
> -----
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> --
> -----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|