Merri,
We have used the 3-1753 for a few years, but mainly by spraying from a
PVA 2000. There have been a few times where we have brushed it on, and
I have had no problems in doing so. The material self levels very
well, and it released any air bubbles it may have had. If you are
brushing over a small area, in small quantities, I do not believe you
will have any problems. You can contact me if you need more
information at [log in to unmask]
Chico Almeras
Diversified Systems
______________________________ Reply Separator _________________________________
Subject: [TN] Conformal Coating
Author: <[log in to unmask]> at Internet-gateway
Date: 3/16/01 12:51 PM
Anyone have experience using Dow Corning 3-1753 Conformal Coating?
This is a silicone, RTV Elastomeric Coating. I am specifically interested
in the 'brush' application method.
Thank you,
Merri Charbonneau
Process Eng.
IFR Americas
--------------------------------------------------------------------------------
-
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet
NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mai
l Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.531
5
--------------------------------------------------------------------------------
-
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|