> Also need input concerning 0603's and glue. Are all you folks having no
> problems placing glue dots under these things with no intrusion into solder
> joints. Asking because I couldn't get it done 2 years ago. If successful,
> what's changed.
>
> Thanks a bunch
How about stenciling the expoxy on Earl? I've done it, works great!
-Steve Gregory-
---------------------------------------------------------------------------------