Hi Guy!
Have you been MicroJoin's web site yet? If not they've got a bunch of *.PDF
articles that are just what you are looking for. Go to:
http://www.microjoin.com/resources/
and click on "reprints", there's a article called: "Hot Bar Soldering
Flex-to-PCB"...
-Steve Gregory-
> Looking for information about direct attach of polyimide flex to rigid FR4.
> Any one out there with knowledge, papers, on the subject of hot bar
> soldering methodology that they can share?
>
> Guy Ramsey
> American Competitiveness Institute
> Senior Lab Technician / Instructor
> 610 362-1200 ext. 107
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------