I responded too quickly. Here is the U.S.A. address.
http://www.dynaloy.com/
Phil
-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: Thursday, March 22, 2001 8:16 AM
To: [log in to unmask]
Subject: Re: [TN] Solvent for RTV738
Jeff,
1) I tried Dynasolve.com and was not taken to their web page.
2) Are you saying that this stuff will dissolve cured or uncured silicones?!
Bev Christian
Research in Motion
-----Original Message-----
From: Gerarden, Jeff [mailto:[log in to unmask]]
Sent: March 22, 2001 2:57 AM
To: [log in to unmask]
Subject: Re: [TN] Solvent for RTV738
If this material is a silicone I have used Dynasolve 225 to dissolve the Dow
Corning RTV on several PCB's with great success. You could find the company
on the web by typing the product name above. Make sure you look at the
technical data sheet on this material. Hope this helps you out.
> Jeff Gerarden
> Focus Factory Supervisor
> PLEXUS-ELECTRONIC ASSEMBLY CORP.
> 2121 Harrison St. Neenah WI 54956
> phone: (920) 751-3226
> email: [log in to unmask]
> http://www.plexus.com
>
>
> -----Original Message-----
> From: <Peter George Duncan> [SMTP:[log in to unmask]]
> Sent: Tuesday, March 20, 2001 8:12 PM
> To: [log in to unmask]
> Subject: [TN] Solvent for RTV738
>
> Hi, TechNetters,
>
> I am trying to find a solvent for removing 3M's RTV 738 that has been used
> for bonding components to a number of boards, or to each other. Any
> suggestions?
>
> I have tried 3M themselves and they have no solvent of their own apart
> from
> "Citrus Base Adhesive Remover" that 'may soften' it enough to peel it off,
> but this seems pretty indefinite.
>
> Thanks in hope
>
> Pete Duncan
> Asst Principal Engineer
> Singapore Technologies Aerospace
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|