Hi, Bob,
What temperature are you at when you give them the cold shower treatment.
Thermal cycling usually ramps at 5 degC/min, but such a cold dose from even
ambient could cause considerable thermal stress that crack any weak joints
you have, and maybe some good ones as well.
My question is, why plunge them into such cold? Are you beaming them out to
Pluto or some other place in the outer darkness?
Rgds
Pete Duncan
Bob Perkins <[log in to unmask]>@IPC.ORG> on 03/21/2001 06:09:44 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Bob Perkins <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] BGA Thermal Cycling and cold spray
Hi all,
I have a question regarding thermal cycling, a good pcb that has passed all
pretests and post tests with a typical thermal cycle. A few PCBs were then
hit with a cold spray of -30c and then tested again, after this test a fall
out of 20%. Are we introducing a crack by the severe thermal shock of the
cold spray or is it revealing a bad solder joint.
Thanks in advance,
Bob Perkins
SMT Process Manufacturing,
Automation Technician
Aimtronics-Delta
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|