Hi Jim,
First, who in God's green earth still uses LLCCs?
Second, how do you define "insufficient joints"?
Third, if you have the same solder volume (are you sure?) and the same pad
size/geometry (make sure), no vias in pad, and solder dams on all the
traces--where did the solder go?
Werner Engelmaier
---------------------------------------------------------------------------------