I noticed the big fat track too, but as it runs right through the ball next
door, and that ball is said to be OK, I took it that it had no effect on
our faulty friend. I asked Rudolph if he had any other microsection
pictures of the surrounding balls for comparison, in case this is another
example of BGA's 'shady tree' effect, as I call it, i.e. the balls sitting
under such a large parasol don't get the heat they need to reflow properly.
Best regs
Pete Duncan
"Stephen R.
Gregory" To: [log in to unmask]
<SteveZeva@AO cc:
L.COM> Subject: Re: [TN] BGA crack pic
Sent by:
TechNet
<[log in to unmask]
ORG>
03/29/01
11:20 AM
Please
respond to
"TechNet
E-Mail
Forum.";
Please
respond to
SteveZeva
Rudolph and everybody,
Go to:
http://www.xdrive.com/share/985835366039lhSi4tEHHweAj9vYGZA6
Good pictures Rudolph! Only thing I notice right away is that big fat trace
next to the ball that's failing...is the same pattern with this device on
the
other boards that you say uses this same asic?
-Steve Gregory-
<< Steve:
Thanks for putting this up for me. So you will let me know the URL
address?
Thanks again
Werner, Peter, Hector:
Thanks for the inputs!!
Rudolph >>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|