>1. How big is a standard sheet of FR4?
USA: 920 x 1220
Asia: 1020 x 1220 (also 1020 x 1020, 920 x 1220, 1060 x 1220)
Germany: 1060 x 1170
Italy: 1060 x 1280
These are standards. Other sizes may be available.