Charles
IMHO, it should be relatively easy to find an answer. What you don't
want is to solder a flex wire to either nickel or stainless steel, as
you will need a fairly active, halogenated flux and this will wick up
the flex, potentially causing corrosion problems at a future date. I
believe the safest way of handling this problem is to pretin the part of
the post where the flex is joined to, using a good, strong water-soluble
flux, which is an easy operation on most stainless alloys, then
thoroughly water wash the posts and then to assemble. You then solder
the flex with a pure rosin flux (or possibly a halide-free "no-clean"
one, with a slightly increased risk).
Brian
[log in to unmask] wrote:
>
> Here is my problem. One of them anyway. We have an assembly with a stainless
> steel pin that has a flex soldered to the end. Currently the pin is nickel
> plated. Due to some problem which has not been explained to me very clearly, it
> has been proposed to eliminate the nickel plate. My problem is obvious. How do I
> solder a little flex to the end of this stainless steel pin? This is a high
> dollar, high reliability assembly. ( Navy pilot wants this to work ) Any
> suggestions or advice are welcome. It may be posssible to have the pin plated
> only on the area that gets soldered but I am looking at the worst case because I
> have been around long enough to know that somebody who does not have to deal
> with a problem can always make it harder on those who do.
> Thanks in advance,
> Charles Caswell
> Process Lead, PCB
> Frontier Electronic Systems
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|