hi,
have you considered the possibility that soldering the first side passivates the nickel on the second side and this inhibits solderability?
phil
-----Original Message-----
From: Mike Bailey [mailto:[log in to unmask]]
Sent: Monday, March 26, 2001 8:01 AM
To: [log in to unmask]
Subject: [TN] Solderability
I could use some thoughts from those of you involved on the assembly side.
We have a customer who appears to have solderability issues with a
particular board we have built. We have supplied this product over the last
several months using three different surface finishes; white tin, HASL and
ENIG. His issue is the same regardless of the surface finish. His first
side produces acceptable solderability however the second side exhibits
non-wetting and partial wetting. I have one of the ENIG boards after
assembly and it shows absolute absence of solder on multiple areas of the
secondary side, while adjacent areas are excellent. I have little specific
information regarding assembly, except as follows:
Screen solderpaste on backside
Inspect
Pick and place components
IR reflow
Aqueous clean
Screen topside with solderpaste
Inspect
Pick & place components
IR reflow
Aqueous clean.
I'm told the customer bakes his boards prior to paste screening, however, I
have no profile specifics etc.
The product in question has no unusual attributes. It's an .062 ten layer
board, no thru-hole, SMT two sides, s single BGA and QFP and the typical
other passives. Process sequence is typical SMOBC with no via plugging etc.
Mike Bailey
Director of Engineering
TTM Technologies
2630 S. Harbor Blvd.
Santa Ana, CA 92704
Phone(714) 241-0303
FAX (714) 241-0708
[log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|