Phil, I agree. In a former life with Ferranti, UK, we used tetra-etch on
many aircraft cables that were to be potted, and cut off the first inch to
be sure of getting conductor that was free of the stuff after immersion.
Brown is good, very brown is very good, especially if it is to perform in
such an acidic environment.
Pete Duncan
Asst Principal Engineer
Singapore Technologies Aerospace
Phil Crepeau <[log in to unmask]>@IPC.ORG> on 03/22/2001 09:08:52 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Phil Crepeau <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: Re: [TN] Potting in PTFE enclosure
hi,
i'm not sure i'm visualizing this properly, but couldn't you cut the wires
longer than you need, tetra-etch the insulation (without immersing the cut
ends into the tetra-etch, and finally trimming them to the desired length?
personally, i'd have a warm feeling if the teflon jacket was brown, because
that would be an indicator that you were going to have a good bond to the
polyurethane potting compound.
phil
-----Original Message-----
From: DUTTON Phil [mailto:[log in to unmask]]
Sent: Wednesday, March 21, 2001 4:03 PM
To: [log in to unmask]
Subject: [TN] Potting in PTFE enclosure
Hello Technetters,
A problem that I hope that some of you assembly experts can help me with.
I have a Printed Board Assy that is to be potted in a PTFE based enclosure.
The wires connecting the board to the outside world are also PTFE
insulated.
The entire unit will spend it's life attached to, and partially immersed in
a lead acid battery. We need a fairly good bond between the potting
compound
(polyurethane)and the PTFE to ensure that none of the corrosive
liquids/vapours can travel by capilliary to the PB. Using a flouropolymer
etch solves this problem, but turns the colour coding on the wires to
brown.
Also there are some concerns about how far the etchant can wick up the
wires, possibly affecting their soldering. A suggestion has been made to
sleeve the wires for a short length, within the encapsulant using adhesive
lined polyolefin heatshrink to provide a seal, rather than etching the
wires. The idea being that the polyolefin will bond to the potting
compound,
and the heatshrink adhesive will bond sufficiently with the PTFE wire
insulation. Is there any problem with this approach, or are there any
suggestions for a better way?
Thankyou,
Phil.
Phil Dutton C.I.D.
Senior CAD Technician
IPC Certified Interconnect Designer
Tenix Defence Systems Pty Ltd
Systems Division - Adelaide
Second Avenue, Technology Park,
Mawson Lakes. SOUTH AUSTRALIA 5095
================================
Phone (08) 8300 4400 (reception)
(08) 8300 4481 (direct)
Fax (08) 8349 7420
email [log in to unmask]
Internet Page http//www.tenix.com
================================
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|