Hi, Steve,
There used to be a time when epoxy ink was ever so gently "shaved off" with
a shiny new scalpel blade. The ink is only ever on the very surface, so can
be done with minimal removal of board material. Otherwise, try contacting
Pelican Inks, who might be able to help.
Rgds
Pete Duncan
"Stephen R. Gregory" <[log in to unmask]>@IPC.ORG> on 03/20/2001 11:36:31 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to [log in to unmask]
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Epoxy Ink Stripper...
Hi ya'll!
Everybody got their "MIR" helmets on? They say now that it'll be Friday
when
they plan to "De-orbit" the space station...
Anyways, could anybody give me a recommendation on a good solvent (or
whatever), to use to remove cured epoxy ink. It's for when there's a
mistake
been made serializing PCB's...
As always, thanks in advance...
-Steve Gregory-
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|