We occasionally cross out the old numbers with epoxy ink and re-number next
to it, as long as you have the real estate. If not, could you scrape it off
using an x-acto knife?
Jim Marsico
Senior Engineer
Production Engineering
AIL/Electronics Systems Group
An EDO Company
[log in to unmask] <mailto:[log in to unmask]>
-----Original Message-----
From: Michael Lester [SMTP:[log in to unmask]]
Sent: Tuesday, March 20, 2001 11:29 AM
To: [log in to unmask]
Subject: Re: [TN] Epoxy Ink Stripper...
We want to get in on this---because we have tried everything from
Ajax to
nitric. What we end up doing is resolder mask the board and then
re-inking
the serial info. It is easier to dissolve the FR4 material than
removing the
cured ink.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|