The classic test for clean Copper should work here...
Put a drop of Silver Nitrate solution, the standard lab 0.1N Silver Nitrate
is fine, on to the Copper. If the Copper is clean, it will turn an
instanteous Black, and the black will not rub off with your finger.
If it is not clean, the black stain will be slow to form, and the resulting
black will be loose, and can be easily rubbed off.
Rudy Sedlak
RD Chemical Company
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|