Ok Industries BGA rework is a division of METCAL and they have a Flux
Transfer Plate that is for that very reason. It uses Past Flux.
Barry Gallegos, PE
Western Electronics, LLC
1550 South Tech Lane
Meridian, Idaho 83642
Phone 208-955-9771
Fax 208-955-9751
-----Original Message-----
From: Trevor Goddard [mailto:[log in to unmask]]
Sent: Monday, February 05, 2001 7:44 AM
To: [log in to unmask]
Subject: [TN] BGA REWORK
Hi all.
I have a question about reworing BGAs. Do you have to reprint the solder
paste before placing the component or can you lay down some flux and rely on
the solder balls of the BGA?
Thanks in advance
Trevor Goddard,
SMT Supervisor
XLTEK
(905) 829-5300 x 348
[log in to unmask] <mailto:[log in to unmask]>
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|