Franklin, I agree that some adjustments must be made to designs to make them
manufacturable, and normally copper areas are increased to allow for
processes, but a 20 mil space down to a 10mil? We only adjust a maximum of
4 mils for 3 oz. etching and we stay within 20% of the design. Sounds like
Robert has a vendor issue to me.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Franklin D Asbell
Sent: Thursday, February 15, 2001 14:57
To: [log in to unmask]
Subject: Re: [TN] design vs reality?
Robert,
Us fabricator type people like to manipulate all that data to suit our
needs, we're evil that way...~evil looking grin~
But seriously, in order to achieve the best yields it is not uncommon
for CAM personnel to make 'adjustments' to gerber in order to make a
product flow more smooth through the fabrication process. It is not
uncommon for clearances to be adjusted to prevent shorts of finished
product. I would expect no more than 1 or 2 mils difference between the
adjusted gerber artwork and finished product, for a process in decent
control.
The plot you're comparing the board to, is this from edited gerber (i.e.
after your fabricator has finished playing with it) or is it the
original design plot?
5 mil difference between artwork and finished board seems an extreme,
unless the fabricator made process adjustments to the gerber.
Franklin
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|