Thanks to all for your support. I already reviewed most of all the
potential root causes (stencil, reflow profile, humidity, temperature,
etc.), but I never reached the "zero defects". My optimum process output
is 38 dpmo's.
I think, when I issued the first question, I did not asked the right
questions:
1. Does somebody has the "perfect" process, where you don't have solder
bridges or insufficient solder?
2. What are your dpmo's, ppm's or % defective?
3. Do you have more or less than 38 dpmo's?
Thanks to all for your support again.
[log in to unmask]
-3com.com To: [log in to unmask],
[log in to unmask]
02/06/01 cc:
08:26 AM Subject: RE: [TN] QFP144 solder bridging
Nicolas,
If the paste looks good after printing and has not bridged or smeared after
the parts are placed, the paste may be 'hot slumping' inside the reflow
oven. You can test this by printing a board and then placing it into an
oven at 100 deg C. for about 10 minutes. If the paste moves significantly,
you have bad solder paste.
Jim Kittel
-----Original Message-----
From: Nicolas Ortiz [mailto:[log in to unmask]]
Sent: Tuesday, February 06, 2001 7:45 AM
To: [log in to unmask]
Subject: Re: [TN] QFP144 solder bridging
Stencil is OK. No changes in design.
Trevor
Goddard To: [log in to unmask]
<tgoddard@XLT cc:
EK.COM> Subject: Re: [TN] QFP144
solder
bridging
Sent by:
TechNet
<[log in to unmask]
ORG>
02/06/01
06:03 AM
Please
respond to
"TechNet
E-Mail
Forum.";
Please
respond to
Trevor
Goddard
Nicolas
I have a couple of questions for you.
Is this a new board or a new Rev of an existing product?
Did you review the stencil design or did you actually have the stencil
measured?
I got caught one time when I was given a new Rev of an existing product.
We
had a couple of QFPs .20mm and a .50mm pitch that were shorting out like
crazy, which was never a problem on the previous Rev. I questioned the guys
that ordered the stencil and the layout guys about what specs the stencil
was ordered to and if there had been a footprint changed. The answers to my
questions was that nothing had changed, but I could still not fix the
problem with process changes. Finally we were able to get the stencil
measured and the pad sizes measured and found out that the apertures on
some
components were 100% of the pad size and another was a tiny bit bigger than
pad size.
My guess is, if nothing has changed in your manufacturing process i.e..
screen printing parameters, reflow profile and your placement is good than
something may have changed in the design side.
Trevor
-----Original Message-----
From: Nicolas Ortiz [mailto:[log in to unmask]]
Sent: Monday, February 05, 2001 3:45 PM
To: [log in to unmask]
Subject: [TN] QFP144 solder bridging
Currently we are experiencing solder bridging on a 0.5mm pitch, LQFP, 144
leads. I already reviewed the stencil design, screen printer parameters and
reflow profile. Everything is OK. We have HASL boards. Our current process
outputs 38 dpmo's. My concern is if I reduce more the apertures, I have the
risk to have solder open or insufficient solder, instead of bridging. Does
anybody has some input? What dpmo's do you have?
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|