Typically I have used limitations such as no more than 3 pads or traces per assembly as long as the pads and traces can be repaired with a high degree of assurrance and per the IPC-7721 guidelines. I have seen other facilities that use the golden number 5 but with no reasoning behind it.
Kathy
>>> [log in to unmask] 02/26/01 03:04AM >>>
Hi! I would like to know if there are any standards or norms as to how many
lifted pads and open traces are allowed for repair within a printed circuit
board. Does anyone know any guidelines to this? I know IPC says that it
depends on the customer, well most customer don't know or don't say. Hope
you guys have more quantitative answers here...
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------