Peter,
Don't believe we have specific documented info regarding the various BGA
rework methods we've tested. I'll also add to comments from Jim Kittel. When
using solder paste vs. flux, or flux paste, you should get better yields
since the paste helps to creates a solder bridge and will account for
co-planarity problems.
Jeff Ferry
-----Original Message-----
From: Peter Loveless, [log in to unmask]
[mailto:[log in to unmask]]
Sent: Monday, February 05, 2001 10:46 AM
To: [log in to unmask]
Subject: Re: BGA REWORK
Jeff,
Has any of your testing been published?
Any chance of getting my hands on your findings?
To: [log in to unmask]
cc:
Subject: Re: [TN] BGA REWORK
Trevor,
We have 4 BGA Reworks systems that go all day. We've tested just about
every
technique possible and apply solder paste vs. flux only in almost every
case.
We've also been using a new type of disposable adhesive backed flexible
stencil for applying the paste that's been a real time saver.
Jeff Ferry
CEO
Circuit Technology Center
www.circuittechctr.com
[log in to unmask]
Chairman
IPC Repairability Committee
-----Original Message-----
From: Trevor Goddard [mailto:[log in to unmask]]
Sent: Monday, February 05, 2001 9:44 AM
To: [log in to unmask]
Subject: BGA REWORK
Hi all.
I have a question about reworing BGAs. Do you have to reprint the solder
paste before placing the component or can you lay down some flux and rely
on
the solder balls of the BGA?
Thanks in advance
Trevor Goddard,
SMT Supervisor
XLTEK
(905) 829-5300 x 348
[log in to unmask] <mailto:[log in to unmask]>
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|