I just picked up on this so my apologies if I duplicate.
What happens if you resolder the board after trimming?
Mike
----- Original Message -----
From: "Bissonnette, Jean-Francois" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, February 07, 2001 12:39 PM
Subject: Re: [TN] fractured joints
> Hi Bob,
>
> I would be concerned about how the leads are trimmed. I've received
boards
> from a vendor who uses some
> kind of rotary cutter (I don't know if the term is right) and
sometimes the
> results are very bad. On a single
> board I've found no less than a dozen fractured joint, all visible
at 6x
> (around 8 to 10% of the leads). These
> devices will also leave partially cut leads which can break loose
and heaven
> knows what can happen than.
>
> My opinion...
>
>
> JF
>
> -----Original Message-----
> From: Bob Arciolla [mailto:[log in to unmask]]
> Sent: Tuesday, February 06, 2001 1:29 PM
> To: [log in to unmask]
> Subject: [TN] fractured joints
>
>
> About two weeks ago I questioned whether clipping leads (and
possible
> fractured joints) was a problem if there was a good fillet on the
component
> side of the board. The main input I received back is that there is a
chance
> of corrousion to the leads. Last week I asked if this would still be
a
> problem if the PCB was totally encapsulated and a vacuum pulled on
the
> units. Any input?????
>
>
>
> WABTEC CORPORATION CONFIDENTIALITY NOTE
> The content contained in this e-mail transmission is legally
privileged and confidential information intended only for the use of
the individual or entity named herein. If the reader of this
transmission is not the intended recipient, you are hereby notified
that any dissemination, distribution, or copying of this transmission
is strictly prohibited.
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|